Fluid Loss Control Additive for Oil Well Cement

Product Description :

G303 can control fluid loss through forming right polymer film and enhancing viscosity of water phase.

Performance Characteristics :

  • Normal dosage: 0.8% ~ 2.0% (BWOC).
  • Slight retarding effect.
  • Suitable temperature: 86℉ ~ 248℉ (BHCT).
  • Low initial consistency and good rheology.
  • No harmful influence on compression strength.
  • Mixed without water.

Technical indicators :

   Appearance powder or particles
   Initial consistency, Bc ≤ 30.0
   Fluid loss, ml / 167℉, 6.9MPa, 30min ≤ 150.0
   Thickening time, min / 167℉, 40MPa, 40min ≥ 60.0
   Compression strength, MPa / 203℉, 21MPa, 24h ≥ 14.0

 

The ingredients of the cement slurry in the table are: G class cement, W/C: 0.44, Dosage of G303: 1.8 % (BWOC), Water quality: distilled water.

Packaging, storage and transportation :

  • Be sacked with three-layer plastics bag, 25kgs per bag.
  • Be kept away from moisture and possible damage of the packages in transportation, and be stored in cool and dry situation.
  • Storage life time is two years.