- G304 consists of many kinds of additives, such as water-soluble polymer.
- Dosage: 0.8% ~ 2.0% (BWOC).
- G304 has a slight irritating smell.
- G304 has a slight retarding effect.
- Applicable temperature range: 30oC ~ 120℃ (BHCT).
- The adding amount should be increased with the increasing temperature, and together with the necessary retarder to adjust thickening time.
- Its initial consistency is small, and slurry rheology is good.
- It has no adverse effect on the compressive strength.
- It’s suitable for dry mixing.
Performance Characteristics :
Technical indicators :
Appearance | Brownish red powder or particles |
Water content, % | ≤ 8.0 |
Fineness (0.315 mm screen residue), % | ≤ 15.0 |
Initial consistency, Bc | ≤ 30.0 |
Thickening liner, min / 80℃, 46.5MPa, 45min | Normal |
Time of 40Bc~100Bc, min | ≤ 40.0 |
Water loss, ml / 80℃, 6.9MPa, 30min | ≤ 150.0 |
Compression strength, MPa / 102℃, 21MPa, 24h | ≥ 14.0 |
The ingredients of the cement in the table are: G class cement, W/C: 0.44, Dosage of G304: 1.2% (BWOC), Water quality: distilled water.
Packaging, storage and transportation :
- Be sacked with three three-layer plastics bag, 25kgs per bag.
- Be kept away from moisture and damaged condition of package during transportation, stored in cool and dry place.
- Storage life time is two years.