- G307B mainly consists of water-dissolved macromolecules, complex with inorganic early strength agent components and other Crystal expandable materials.
- Normal dosage: 2.0% ~ 3.5% (BWOC).
- G307Bcan effectively enhance the early strength of cement stone.
- It has the micro-expansion effect, and can effectively compensate for pressure loss caused by the hydration volume reduction, thus effectively preventing the gas-water leaking in the stratum.
- Applicable temperature:30℃ ~ 90℃ (BHCT).
- Combined with retarder, can be used in shallow-deep and middle-deep wells.
- Preferred to mix without water.
Early Strength and Anti leaking Fluid Loss Control Additive
Product Description :
G307B Early Strength and Anti leaking Fluid Loss Control Additive for Oil Well Cement belongs to Water-soluble high polymer. Molecular chains get together in the cement slurry, thus to reduce the penetration ratio of slurry cake. In addition, drawing a variety of functional groups into the polymer will enhance the product’s dissolution rate and the performance of anti-high-temperature and anti-salt at a low temperature in the cement slurry.
Performance Characteristics :
Technical indicators :
Appearance | Floating powder or particles |
Water content, % | ≤ 8.0 |
Fineness (0.315 mm screen residue), % | ≤ 15.0 |
Initial consistency, Bc / 50℃, 25.9MPa, 32min | ≤ 30.0 |
Thickening liner | Normal |
Time of 40Bc ~ 100Bc, min | ≤ 40.0 |
Water loss, ml / 50℃, 6.9MPa, 30min | ≤ 150.0 |
Compression strength, MPa / 71℃, 21MPa, 24h | ≥ 14.0 |
The ingredient of the cement slurry in the table is: G class cement, W/C: 0.44, Dosage of G307B: 2.5 % (BWOC), Water quality: distilled water.
Packaging, storage and transportation :
- Be sacked with three three-layer plastics bag, 25kgs per bag.
- Be kept away from moisture and damaged condition of package during transportation, stored in cool and dry place.
- Storage life time is two years.