Early Strength Additive for Oil Well Cement

Product Description :

By changing the structure of C-S-H, G203A can transform the composition of water phase ion, thus to reach the goal of accelerating cement hydration and enhancing early strength of cement stones.

Performance Characteristics :

  • G203A is made from inorganic materials.
  • Normal dosage: 1.0%~4.0% (BWOC).
  • Increase early strength of cement stones efficiently and has no harmful influence on later strength increasing.
  • Suitable for oil / gas wells whose temperature is between 30℃~90℃ (BHCT).
  • Shorten the thickening time of cement slurry effectively and enhance the early strength of cement stone.
  • It makes cement slurry with a slight thixotropy when mixed with G203A.

Technical indicators :

Appearance White or light yellow powder
Water Content, % ≤ 8.0
Fineness ( 0.315 mm screen residue ), % ≤ 15.0
Initial consistency, Bc ≤ 30.0
Thickening time, min / 60℃, 25MPa ≤ 60.0
Compression strength, MPa / 60℃, Normal pressure 8 h ≥ 8.0
24 h ≥ 20.0

 

The ingredient of normal cement slurry in the table is: G class cement, W/C: 0.44, Water quality: distilled water, Dosage of G203A: 2.0% (BWOC).

Packaging, storage and transportation :

  • Be packed with three-layer plastic bags, 25kg per bag.
  • Be kept away from moisture in transportation. If moistened, the additive dosage should be increased. It should be mixed with water when it is used. The worker should wear protective stuff to avoid contacting with skin while operating.
  • The storage life time is two years.