GH-6 consists of various kinds of compounds, such as gluconate and
hydroxycarboxylic acid.
Non-poisonous, non-odor, and non-corrosivity.
Normal dosage: 0.06% ~1.0% ( BWOC ). The amount can be appropriately
increasea with the increase of temperature.
It can reduce the consistency of cement slurry and improve the rheology.
Retard the thickening time efficiently.
Generally used in oil wells whose circulate temperature under bore is between
75℃ to 110℃.
GH-6 is sensitive, so the dosage should be accurately measure.
Items | Specification |
Appearance | Colorless transparent liquid |
Density, g/cm3 ( 20 ± 1℃ ) | 1.09 ~ 1.15 |
Thickening time / 80℃, 46.5MPa, 45min | ≥ 120.0 |
Initial consistency, Bc | ≤ 30.0 |
Mutation value of thickening curve, Bc | ≤ 10.0 |
Thickening time extension value, min | ≥ 60.0 |
Sensitivity of increase, % | ≤ 25.0 |
Sensitivity of temperature, % | ≤ 20.0 |
Transition time, min | ≤ 40.0 |
Free liquid, % | ≤ 1.4 |
Compression strength, MPa / 102℃, 21MPa, 24h | ≥ 14.0 |
The ingredient of the cement slurry in the table is: JiaHua G class: cement , W/C 0.44, Dosage of GH-6: 0.1%, 0.5% USZ ( BWOC ), 0.5% G301 ( BWOC ), Water quality: distilled water.
Be stored in 25L plastic barrels, 25kg per barrel.
Be kept away from moisture and possible damage of the packages in
transportation, be stored in cool and dry situation.
Storage life time is one year.