Fluid Loss Control Additive for Oil Well Cement

Product Description :

G303 can control fluid loss through forming right polymer film and enhancing viscosity of water phase.

Performance Characteristics :

Normal dosage: 0.8% ~ 2.0% (BWOC).

Slight retarding effect.

Suitable temperature: 86℉ ~ 248℉ (BHCT).

Low initial consistency and good rheology.

No harmful influence on compression strength.

Mixed without water.

Technical indicators :

   Appearancepowder or particles
   Initial consistency, Bc≤ 30.0
   Fluid loss, ml / 167℉, 6.9MPa, 30min≤ 150.0
   Thickening time, min / 167℉, 40MPa, 40min≥ 60.0
   Compression strength, MPa / 203℉, 21MPa, 24h≥ 14.0

 

The ingredients of the cement slurry in the table are: G class cement, W/C: 0.44, Dosage of G303: 1.8 % (BWOC), Water quality: distilled water.

Packaging, storage and transportation :

Be sacked with three-layer plastics bag, 25kgs per bag.

Be kept away from moisture and possible damage of the packages in transportation, and be stored in cool and dry situation.

Storage life time is two years.