G203A is made from inorganic materials.
Normal dosage: 1.0%~4.0% (BWOC).
Increase early strength of cement stones efficiently and has no harmful
influence on later strength increasing.
Suitable for oil / gas wells whose temperature is between 30℃~90℃ (BHCT).
Shorten the thickening time of cement slurry effectively and enhance the
early strength of cement stone.
It makes cement slurry with a slight thixotropy when mixed with G203A.
Appearance | White or light yellow powder |
Water Content, % | ≤ 8.0 |
Fineness ( 0.315 mm screen residue ), % | ≤ 15.0 |
Initial consistency, Bc | ≤ 30.0 |
Thickening time, min / 60℃, 25MPa | ≤ 60.0 |
Compression strength, MPa / 60℃, Normal pressure | 8 h | ≥ 8.0 |
24 h | ≥ 20.0 |
The ingredient of normal cement slurry in the table is: G class cement, W/C: 0.44, Water quality: distilled water, Dosage of G203A: 2.0% (BWOC).
Be packed with three-layer plastic bags, 25kg per bag.
Be kept away from moisture in transportation. If moistened, the additive
dosage should be increased. It should be mixed with water when it is used. The
worker should wear protective stuff to avoid contacting with skin while
operating.
The storage life time is two years.